1-14 of 14 Search Results for

No. 484 TOOL STEEL

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1990) 39 (6): TS-501.
Published: 01 June 1990
... No. 484 tool steel is an air hardening tool steel capable of through hardening in heavy sections. Isothermal transformation of material austenitized at 1750 starts after about 400 seconds at 1300 F and after about 1000 seconds at 600 F. The calculated Ms temperature is 325 F. The steel has a good...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1987) 36 (11): TS-484.
Published: 01 November 1987
... elasticity fracture toughness hardness heat treatability high-temperature alloys machinability physical properties punch tools shock resistance workability AL mcH B47 Filing Code: TS-484 Tool Steel NOVEMBER 1887 - DATA ON WORLD WIDE METALS AND ALLOYS 0 copyright 1987. Alloy Di#en. Inc. Au ri@m...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1997) 46 (1): SA-484.
Published: 01 January 1997
... Lukens MTD steels are prehardened alloy plate steels developed for mold, tool, and die applications. This datasheet provides information on composition and hardness. It also includes information on heat treating, machining, and joining. Filing Code: SA-484. Producer or source: Lukens Steel Company...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1964) 13 (8): TS-150.
Published: 01 August 1964
... Seneca Hot Die is a tungsten-chromium-vanadium type hot work steel having good red hardness and abrasion resistance. It is recommended for forging dies, copper extrusion dies, die casting dies, and other hot work tools and dies. This datasheet provides information on composition, physical...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1955) 4 (5): TS-33.
Published: 01 May 1955
... JESSOP 2-B machinability workability Filing Code: TS-33 JESSOP 2=B Tool Steel MAY 1955 - DATA ON WORLD WIDE METALS AND ALLOYS Pnblisbd br Engineering Alloys Di.mr. Irk. Upper Montclair. New Jrrscv JESSOP 2-B (Hot Work Die Steel) JESSOP 2-B is a general purpose hoc work die steel having great...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1975) 24 (7): SS-314.
Published: 01 July 1975
... Mootchir, New Jersey CRUCIBLE CSM 420 (DENSI FI ED* Stainless Mold Steel for Plastics; Cross Reference to Tool Steels) CRUCIBLE CSM 420 is furnished in the annealed condition and designed primarily for use in the molding of all plastics, including the vinyl-base and other corrosive plastics. Crucible s...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1965) 14 (8): TS-168.
Published: 01 August 1965
... AISI Type-A2 is a high-carbon, chromium, molybdenum tool and die steel having excellent non-deforming properties, abrasion resistance, toughness and good machinability. It is used for blanking and forming dies, rolls, punches, gauges, broaches, etc. This datasheet provides information...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1984) 33 (5): SS-445.
Published: 01 May 1984
... by any thermal treatment. It can be hardened and strength- ened only by cold working. Machinability: Avesta 254 SMOcan be machined by the conventional methods used for austenitic stainless steels. It is important to keep the tool continually entering the work to avoid work hardening the surface...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1981) 30 (7): SA-382.
Published: 01 July 1981
... SAE 8642 is a triple-alloy steel that can be hardened by austenitizing and quenching in oil. This steel has moderate hardenability with relative high strength and toughness, especially in the quenched-and-tempered condition. It is used in a wide range of components, parts and tools; examples...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1989) 38 (10): SA-440.
Published: 01 October 1989
... AISI 8642 is a triple-alloy steel that can be hardened by austenitizing and quenching in oil. This steel has moderate hardenability with relatively high strength and toughness, especially in the quenched-and-tempered condition. It is used in a wide range of components, parts and tools; examples...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1987) 36 (4): SS-484.
Published: 01 April 1987
... as deformation, and fatigue. It also includes information on high temperature performance as well as forming, heat treating, machining, and joining. Filing Code: SS-484. Producer or source: Armco Inc., Specialty Steels Division. Producer or Source: Armco Inc., Specialty Steels Division Copyright © ASM...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1978) 27 (7): Co-20.
Published: 01 July 1978
... chemical composition compressive strength cutting tools elasticity HAYNES STELLITE ALLOY No. 6K heat treatability joinability machinability physical properties wear resistance workability Au Filing Code: Co-20 cobalt Alloy Or HAYNES STELLITE Alloy No. 6K Revised JULY 1979 MAY 1999 DIQEST...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1961) 10 (11): Ni-68.
Published: 01 November 1961
... is satisfactorily mschinsd. Because of its toughoess, cutting speeds are somewhat slower and feeds lighter than those for mild sreel. Tools should be of tungsten high-speed steel or super (cobalt) high-speed steel, ground with sbsrper angles dran for carbon steel. Tungsten or titanium carbide tools may also be used...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2020) 69 (10): SS-1328.
Published: 01 October 2020
... than mild steel and tends to harden rapidly during working. The chips produced are stringy and tough and retain considerable duc- tility. Tooling should be kept sharp and be rigidly held. Deeper cuts and slower speeds are generally used to cut below work hardened zones. Due to the low thermal con...