Alloy Digest (2005) 54 (6): SS-931.
Published: 01 June 2005
... Carlson alloy Nitronic 33 has twice the yield strength of 304 stainless with comparable corrosion resistance. The low magnetic permeability of the alloy is retained after severe cold working. The resistance to chloride stress-corrosion cracking is superior to Type 304. Nitronic 33 has excellent...
Journal Articles
Alloy Digest (2013) 62 (4): SS-1142.
Published: 01 April 2013
... Electralloy’s Nitronic 33 is a nitrogen strengthened austenitic stainless steel. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on corrosion and wear resistance as well as forming, heat treating, machining, and joining...
Journal Articles
Alloy Digest (2018) 67 (10): SS-1295.
Published: 01 October 2018
... Electralloy Nitronic 33 was created with a high-yield strength, excellent toughness, and ductility. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well...
Journal Articles
Alloy Digest (1976) 25 (1): SS-324.
Published: 01 January 1976
... NITRONIC 33 is characterized by (1) High yield strength, (2) Good resistance to stress-corrosion cracking, (3) Low magnetic permeability even after severe cold working, (4) Excellent strength and ductility at cryogenic temperatures, and (5) Good resistance to wear and galling; in fact...
Journal Articles
Alloy Digest (1998) 47 (6): SS-721.
Published: 01 June 1998
... Electralloy Nitronic 60 is an alloy with excellent uniform corrosion resistance, outstanding galling resistance, high strength, and good high-temperature oxidation resistance. The alloy retains toughness at low temperature. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1992) 41 (8): SS-533.
Published: 01 August 1992
... NITRONIC 30 is a nitrogen-strengthened stainless steel with a good combination of strength, corrosion and wet abrasive wear resistance and economy. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness...
Journal Articles
Alloy Digest (1998) 47 (5): SS-715.
Published: 01 May 1998
... Electralloy Nitronic 50 provides a combination of corrosion-resistance wear and strength not found in other stainless steels. High-speed (HS) Nitronic 50 has a yield strength that is 3 to 4 times that of type 316 stainless steel. This datasheet provides information on composition and physical...
Journal Articles
Alloy Digest (2009) 58 (2): SS-1029.
Published: 01 February 2009
... CARLSON ALLOY NITRONIC 60 is a galling- and wear-resistant austenitic stainless steel that provides a significantly lower-cost alternative to cobalt-bearing and high-nickel alloys. Corrosion resistance is superior to 304 in most media. Approximately twice the yield strength of 340 and 316...