Alloy Digest (1974) 23 (6): SA-305.
Published: 01 June 1974
... Nitriding BM is a free-cutting grade of nitriding steel that can be surface hardened by the standards nitriding processes. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as...