Alloy Digest (1955) 4 (12): CI-13.
Published: 01 December 1955
... NITRICASTIRON is a chromium, aluminum, molybdenum iron having a surface capable of being hardened to a high degree in an atmosphere of ammonia at temperatures below 1000 F. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties...