1-3 of 3 Search Results for

Nitralloy 230

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1961) 10 (11): SA-122.
Published: 01 November 1961
... NITRALLOY 230 is a special alloy steel which can be nitrided, that is, surface hardened, without final quenching, by the action of partially dissociated ammonia gas at temperatures from about 925-1025 F. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (1957) 6 (9): SA-61.
Published: 01 September 1957
... NITRALLOY 125 (0.20-0.30% C) is a special alloy steel which can be nitrided, that is, surface hardened, without final quenching, by the action of ammonia gas at relatively low temperatures. Nitralloy 125 is also known as Nitralloy H. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1956) 5 (10): SA-48.
Published: 01 October 1956
... Specific hear, BTU/lbF. 2bdenum Electrical resistance, microhm-cm Remainder Modulus of elasticity, psi +Registered Trade Mark, The Nitralloy Corporation, 230 Park Ave., New York, N. Y. PROPERTIES Tempering Temperature, OF. 800 900 1000 1100 2 ::i: TYPICAL CORE PROPERTIES (Oil quenched from 1650┬░F...