Alloy Digest (2007) 56 (4): Ni-648.
Published: 01 April 2007
... Nistelle Super C is a nickel-base powder metallurgy alloy designed for corrosion resistance and developed for coating and overlaying purposes. The composition of Nistelle Super C, Ni-23Cr-18Mo, is similar to that of the traditional Nistelle alloy, which is Ni-16Cr-16Mo-4.5W, but the higher...