Alloy Digest (1969) 18 (10): Fe-39.
Published: 01 October 1969
... Niromet 46 is a 46% nickel-iron alloy having low and controlled coefficient of expansion. It is recommended for metal-to-glass seals and terminal bands in vitreous enameled resistors. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also...