Alloy Digest (2017) 66 (12): Ni-740.
Published: 01 December 2017
... Nippon Sumitomo Super625 is a nickel alloy with an optimization of compositional elements for thermal stability and hot workability. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness. It also includes...