Alloy Digest (2003) 52 (3): Ni-603.
Published: 01 March 2003
... Metrode Nimrod AKS and AB, and Nimax A are nickel-base consumables similar to 182, but with lower manganese and with a molybdenum addition. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness. It also includes information on joining...
Journal Articles
Alloy Digest (2003) 52 (1): Ni-599.
Published: 01 January 2003
..., this consumable is suitable for welding heat-resistant alloys including Inconel 601 (except in severe sulfidizing condi- tions), Incoloy 800/800H (preferred to Nimrod AKS above about 900 °C, or 1652 °F) or combinations of these with other alloys for furnace equipment, petrochemical, and power- generation plants...