Alloy Digest (2002) 51 (12): Ni-596.
Published: 01 December 2002
... Nimrod 59KS is a basic all-positional pipe-welding electrode for Alloy 59 (see NICROFER 5923 hMo, Alloy Digest Ni-430, May 1993) and other highly corrosion-resistant alloys with very high molybdenum content. This datasheet provides information on composition and tensile properties as well...