Alloy Digest (1996) 45 (4): Ni-339.
Published: 01 April 1996
... Nimonic alloy 901 is a nickel-base alloy strengthened by additions of molybdenum, titanium, and aluminum. It possesses high creep and rupture strength from 1000 to 1400 deg F. Applications include components for gas turbines, bolting, and valve stems for power applications. This datasheet provides...