Alloy Digest (1996) 45 (3): Ni-503.
Published: 01 March 1996
... NIMONIC alloy 91 is a modification of NIMONIC alloy 90 (Alloy Digest Ni-6, December 1961) with better stability and improved hot corrosion resistance. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes...
Journal Articles
Alloy Digest (1996) 45 (4): Ni-339.
Published: 01 April 1996
... Nimonic alloy 901 is a nickel-base alloy strengthened by additions of molybdenum, titanium, and aluminum. It possesses high creep and rupture strength from 1000 to 1400 deg F. Applications include components for gas turbines, bolting, and valve stems for power applications. This datasheet provides...
Journal Articles
Alloy Digest (1954) 3 (5): Ni-10.
Published: 01 May 1954
... Nimonic 80 and Nimonic 80A are nickel-base alloys containing a high percentage of chromium, with aluminum and titanium as hardening agents. They are made to the same compositional specification, but Nimonic 80A is produced to meet a more severe requirement with respect to resistance to creep when...
Journal Articles
Alloy Digest (1956) 5 (1): Ni-22.
Published: 01 January 1956
... NIMONIC 75 is basically an 80/20 nickel-chromium alloy combining inherent oxidation resistance with high mechanical properties at elevated temperatures. It is amenable to all forms of fabrication and welding. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1958) 7 (1): SS-67.
Published: 01 January 1958
... NIMONIC DS is a wrought, austenitic nickel-chromium-iron alloy having high oxidation and heat resistance. It is recommended for furnace parts and gas turbine components. This datasheet provides information on composition, physical properties, and elasticity as well as creep. It also includes...
Journal Articles
Alloy Digest (1970) 19 (5): Ni-153.
Published: 01 May 1970
... NIMONIC 93 is a nickel-base alloy having high elevated temperature strength, high oxidation resistance and good corrosion resistance. It is recommended for jet engine and gas turbine components. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (1987) 36 (2): Ni-345.
Published: 01 February 1987
... NIMONIC Alloy 81 is a wrought nickel alloy designed to provide enhanced resistance to high-temperature corrosion coupled with good high-temperature strength. It is particularly resistant to attack by deposits of alkali metal sulfates and chlorides resulting from combustion of impure fuels...
Journal Articles
Alloy Digest (1987) 36 (7): Ni-350.
Published: 01 July 1987
... NIMONIC Alloy 263 is an air-melted nickel-base alloy which has improved ductility in welded assembly. Developed originally as a sheet material, it is available in all standard forms. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well...
Journal Articles
Alloy Digest (1987) 36 (9): Ni-351.
Published: 01 September 1987
... NIMONIC alloy 86 is a nickel-base high-temperature alloy with exceptionally good cyclic oxidation resistance at 1050 C (1922 F). The alloy has good workability, ductility and weldability. It is intended principally for use in sheet form. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1967) 16 (10): Ni-128.
Published: 01 October 1967
... NIMONIC 110 is a highly alloyed nickel-base alloy having high creep and oxidation resistance. It is recommended for aircraft gas turbine components to resist the stresses at the very high temperatures of operation. This datasheet provides information on composition, physical properties, elasticity...
Journal Articles
Alloy Digest (1961) 10 (12): Ni-6.
Published: 01 December 1961
... NIMONIC 90 is a nickel-base alloy containing high percentages of chromium and cobalt with aluminum and titanium as hardening agents. It has strength at high temperature levels, and is highly resistant to scaling, oxidation, heat and corrosion. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1991) 40 (4): Ni-393.
Published: 01 April 1991
... AND ALLOYS APRIL 1991 P-by: Aloy Mgeg. k1201-677.9161 Z.7Canfbld9tmeCOrangaNJ.OMX)IU.S.A ALLVAC 90 (Precipitation-Hardening, High-Temperature Nimonic Alloy) ALLVAC 90 is a nickel-base alloy containing cobalt to provide improved tensile and creep-rupture properties up to 16oooF (871OC) and chromium...
Journal Articles
Alloy Digest (1991) 40 (5): Ni-66.
Published: 01 May 1991
... NIMONIC ALLOY 105 is a wrought nickel-cobalt-chromium-base alloy strengthened by additions of molybdenum, aluminum and titanium. It has been developed for service up to 950 C (1742 F). This datasheet provides information on composition, physical properties, and elasticity as well as creep. It also...
Journal Articles
Alloy Digest (1991) 40 (11): Ni-104.
Published: 01 November 1991
... NIMONIC alloy 115 is a nickel/chromium/cobalt based alloy developed as a vacuum processed creep resisting alloy for service at temperatures up to about 1010 C (1850 F) as a turbine blade material for aircraft turbines. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (2005) 54 (7): Ni-626.
Published: 01 July 2005
... Nimonic alloy PK33 is a nickel-base aerospace alloy developed to produce sheet with ultrahigh strength and good formability. This datasheet provides information on composition, physical properties, hardness, tensile properties, and shear strength as well as creep. It also includes information...
Journal Articles
Alloy Digest (2017) 66 (3): Ni-728.
Published: 01 March 2017
... Nimonic PE11 is a nickel-iron-chromium alloy that is precipitation hardened. It is used at high temperatures. This datasheet provides information on composition and physical properties. It also includes information on high temperature performance as well as forming. Filing Code: Ni-728. Producer...
Journal Articles
Alloy Digest (1986) 35 (7): Ni-334.
Published: 01 July 1986
... NIMOCAST Alloy 80 is the casting counterpart of NIMONIC Alloy 80A (Alloy Digest Ni-10, May 1954). It may be used as as cast but develops optimum mechanical properties in the fully heat treated condition. NIMOCAST Alloy 80 is used for diesel engine precombustion chambers and for other high...
Journal Articles
Alloy Digest (2003) 52 (9): Ni-613.
Published: 01 September 2003
... (1400 °F). Maximum hardness is attained in 12 h. Fabricability: Alloy 740 is readily fabricated in the annealed condition. Weldability: Joining is accomplished with the gas tungsten arc welding (GTAW) process using Nimonic Filler Metal 263. If a high joint strength is required, the deposited weldment...
Journal Articles
Alloy Digest (2003) 52 (5): Ni-607.
Published: 01 May 2003
..., and 330, Nimonic 75, and ASTM cast grade CY40 in A494. The electrodes are stored in three hermetically sealed ring-pull metal tins per carton, with unlimited shelf life. Direct use from tin is satisfactory for much longer than an 8 h working shift. For elec- trodes that have been exposed, redry at 200 205...
Journal Articles
Alloy Digest (2021) 70 (2): Ni-767.
Published: 01 February 2021
...·°F)) 20 °C (6.47)(a) resistivity (68 °F) J/(kg K) 448 (cal/(g °C)) (0.107)(a) m 1.24 circular-mil/ft) (746)(a) For coefficient of linear thermal expansion see Fig. 1. (a) Source: Nimonic 80A, Special Metals Corporation Mechanical Properties Tensile Properties. See Fig. 2 and 3. Hardness. The hardness...