Alloy Digest (2002) 51 (6): Ni-498.
Published: 01 June 2002
... Nimofer 6629, also called alloy B-4, is a 28 molybdenum alloy with low interstitials and a balanced chemistry to suppress beta-phase formation during thermo-mechanical operations. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties...