Journal Articles
Alloy Digest (1997) 46 (1): Ni-520.
Published: 01 January 1997
... Nicrofer 7216 H is a solution-treated nickel-chromium-iron alloy with good resistance to oxidation, carburization, and nitriding; good resistance to stress-corrosion cracking; and good resistance to dry chlorine and hydrogen chloride. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (2001) 50 (6): Ni-568.
Published: 01 June 2001