Alloy Digest (1994) 43 (5): Ni-452.
Published: 01 May 1994
... NICROBRAZ LM is a low melting general-purpose brazing filter metal for applications requiring high joint strength and oxidation resistance up to 2200 F. This datasheet provides information on composition and physical properties. It also includes information on corrosion resistance as well...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2003) 52 (9): Ni-614.
Published: 01 September 2003
... strength. The most reliable tests for design purposes are stress rupture or simulated service tests. In the manufacture of plate-and-fin type of heat exchangers, Nicrobraz 31 has exceeded the strength of Nicrobraz LM (AMS 4777, AWS BNi-2) and Nicrobraz 30 (AMS 4782, AWS BNi 5) brazed heat exchangers. Burst...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1997) 46 (2): Ni-522.
Published: 01 February 1997
...). Corrosion Resistance: Nicrobraz 110 is a modified Nicrobraz LM tiller metal with improved corrosion resistance. To obtain the best cotrosion-resis- tam proper&. brazing should be executed at the lowest suitable brazing kmpemmm for the shortest time at heat A second pro cedure involves holding at the brazing...