Alloy Digest (1994) 43 (10): Ni-468.
Published: 01 October 1994
... NICROBRAZ 130 is a good general-purpose filler metal. It flows freely in marginal atmospheres, in deep or tight joints. This datasheet provides information on composition, physical properties, and hardness. It also includes information on corrosion resistance as well as joining. Filing Code: Ni...
Journal Articles
Alloy Digest (1997) 46 (4): Ni-525.
Published: 01 April 1997
... Nicrobraz is a free-flowing nickel brazing filler metal with a wide melting range and low diffusion with most base metals. The brazing metal meets AWS, AMS, G.E., and other specifications. This datasheet provides information on composition, physical properties, and hardness. It also includes...