Alloy Digest (1994) 43 (3): Ni-448.
Published: 01 March 1994
... NICROBRAZE 10 is a free flowing, low melting, chromium-free filler metal, good for marginal atmospheres. It minimizes base metal erosion during the brazing operation. This datasheet provides information on composition and physical properties. It also includes information on joining. Filing Code...
Journal Articles
Alloy Digest (2003) 52 (9): Ni-614.
Published: 01 September 2003
... Nicrobraz 31 is a high-chromium, oxidation-resistant nickel braze filler metal with enhanced flow properties. This datasheet provides information on composition. It also includes information on corrosion resistance as well as joining. Filing Code: Ni-614. Producer or source: Wall Colmonoy...
Journal Articles
Alloy Digest (2009) 58 (10): Ni-674.
Published: 01 October 2009
... Nicrobraz 152 is a high-chromium, oxidation-resistant nickel brazing filler metal with enhanced flow properties. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on corrosion resistance as well as forming, joining...
Journal Articles
Alloy Digest (1994) 43 (9): Ni-462.
Published: 01 September 1994
... NICROBRAZ 51 is a low-melting, free-flowing filler metal similar to Nicrobraz 50 except for greater strength, and heat and corrosion resistance. This datasheet provides information on composition and physical properties. It also includes information on corrosion resistance as well as joining...
Journal Articles
Alloy Digest (2009) 58 (11): Co-118.
Published: 01 November 2009
... Nicrobraz 210 is a Co-Cr-Ni-W nickel brazing filler metal with enhanced strength at high temperatures and low base metal penetration. This datasheet provides information on composition and hardness. It also includes information on high temperature performance and corrosion resistance as well...
Journal Articles
Alloy Digest (1995) 44 (2): Ni-478.
Published: 01 February 1995
... NICROBRAZ 171 is a base filler metal with extra high strength at temperature. It is good for brazing base metals containing cobalt, tungsten, and molybdenum and has a better flow characteristic than Nicrobraz 170 (Alloy Digest Ni-476, January 1995). This datasheet provides information...
Journal Articles
Alloy Digest (1995) 44 (1): Ni-476.
Published: 01 January 1995
... NICROBRAZ 170 is an extra high strength at high temperature braze filler metal. It is good for brazing nickel-base materials containing cobalt, tungsten, and molybdenum. This datasheet provides information on composition, physical properties, and hardness. It also includes information on corrosion...
Journal Articles
Alloy Digest (1994) 43 (3): Cu-597.
Published: 01 March 1994
..., flow, and drying properties, and vaporizes completely under furnace heat. There is a binding agent which gives a dry strength to applied powder similar to that imparted by Nicrobraz Cement. The vehicle is non-flammable, non- toxic, and odor&e. Special ventilation is not required in the area where...