1-20 of 1999 Search Results for

Nickel-200

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1998) 47 (6): Ni-539.
Published: 01 June 1998
... Nickel 200 and Nickel 201 are wrought metals of commercially pure nickel that are used in specific corrosive service, such as caustic alkali environments, or for their unique physical properties, particularly in the electronics industry. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1977) 26 (6): Ni-246.
Published: 01 June 1977
... TECHALLOY Nickel 200 is commercially pure wrought nickel. It maintains good strength at elevated temperatures and is tough and ductile at low temperatures. It is a general-purpose material when the properties of nickel alloys are not needed. Its many uses include spun and cold-formed parts...
Journal Articles
Alloy Digest (1962) 11 (10): Ni-75.
Published: 01 October 1962
... Nickel-200 is a wrought metal combining excellent mechanical properties with corrosion resistance. It retains its strength to an excellent degree at high temperatures. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as...
Journal Articles
Alloy Digest (1985) 34 (6): Ni-316.
Published: 01 June 1985
... Nickel Welding Electrode 141 is used for shielded-metal-arc welding of Nickel 200 and Nickel 201, welding the clad side of nickel-clad steel and surfacing of steel. This electrode also is used for dissimilar welding, including joints between Nickel 200 and 201 and various iron-base and nickel-base...
Journal Articles
Alloy Digest (1986) 35 (8): SA-422.
Published: 01 August 1986
... VascoMax T-200 is an 18% nickel maraging steel with titanium as the primary strengthening agent and containing no cobalt. It is double vacuum melted to assure high purity which is essential for optimum mechanical properties. Price stability is an advantage with titanium-strengthened maraging...
Journal Articles
Alloy Digest (1982) 31 (12): Ni-281.
Published: 01 December 1982
... properties thermal conductivity workability UNS N02200 Filing Code: Ni-2&l RA 200 Nickel %I DECEMBER 1982 MCIsr - DATA ON WORLD WIDE METALS AND Al.LoYs p-by @ Copyright 1980, Engineering Publications. IIK. WI righti mSWWd. ISSN: 002-614x -Yt2%Ezh% Inc Uppa Meotdair, New jersey RA 200* (Commercially...
Journal Articles
Alloy Digest (1988) 37 (11): Ni-364.
Published: 01 November 1988
... AL 200 and AL 201 alloys are wrought commercially pure nickel. They differ, as to composition, in maximum specified carbon levels (0.15 for AL 200 and 0.02 for AL 201). Strengths of both alloys in the annealed condition are similar to that of mild steel. The lower carbon AL 201 alloy has higher...
Journal Articles
Alloy Digest (1960) 9 (6): SA-99.
Published: 01 June 1960
.... New Jm JESSOP No. 200 (Manganese-Nickel Alloy Steel I JESSOP No. 208 is a non-magnetic, austenitic steel developed especially for the electrical industry. It has low magnetic per- meability and high electrical resistance. Jessop NO. 200 is ideal for a great number of applications requiring low perme...
Journal Articles
Alloy Digest (1985) 34 (1): Ni-308.
Published: 01 January 1985
... Nickel Filler Metal 61 is a nickel-base alloy that is used for welding Nickel 200 and Nickel 201 to themselves and to other alloys such as stainless steel, carbon steels, copper-nickel alloys, INCONEL alloys, INCOLOY alloys and MONEL alloys. The weld metal has moderate strength and ductility and...
Journal Articles
Alloy Digest (1977) 26 (8): Ni-248.
Published: 01 August 1977
... TECHALLOY Nickel 211 is a nickel-manganese alloy with good elevated-temperature resistance to corrosion by sulfur compounds. When annealed, it is slightly stronger and harder than Techalloy Nickel 200 and is good for structural parts subjected to degassing temperatures. Nickel 211 has low electron...
Journal Articles
Alloy Digest (1985) 34 (5): Ni-315.
Published: 01 May 1985
... and Nickel 200 to stainless steels and (3) Joining stainless steels to carbon steels. This filler metal also is used for welding nickel steels. This datasheet provides information on composition and tensile properties. It also includes information on corrosion resistance as well as forming, heat...
Journal Articles
Alloy Digest (1988) 37 (9): Ni-361.
Published: 01 September 1988
... CARPENTER NICKEL 211 ALLOY is a nickel-manganese alloy that is slightly harder than commercially pure nickel (Nickel 200). It is a solid-solution strengthened alloy. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on...
Journal Articles
Alloy Digest (1968) 17 (10): Ni-139.
Published: 01 October 1968
... NICKEL 201 is a low carbon version of Nickel 200 recommended for use in the electronic industries for service at temperatures between 600 F and 1200 F. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes...
Journal Articles
Alloy Digest (1969) 18 (6): Cu-200.
Published: 01 June 1969
... corrosion-resistant alloys CUPRO NICKEL 30%-716 elasticity feedwater heater heat exchanger tubes joinability physical properties tensile properties workability 1 ~~ CUpRf) NICKEL, 3716 cu-200 JUNE 1999 DIGEST d - DATA ON WORLD WIDE METALS AND ALLOYS Publisbd by Engineering Alloys Digest, Inc...
Journal Articles
Alloy Digest (1974) 23 (2): Ni-200.
Published: 01 February 1974
... toughness hardness heat resistance heat treatability machinability oxidation resistance physical properties powder metal products tensile properties Au OB AWRY 761 Filing Code: Ni-200 Nickel Alloy FEBRUARY 1974 DIGESTd - DATA ON WORLD WIDE METALS AND ALLOYS . +blisbd by EncpocenneAlloyrDigat,I...
Journal Articles
Alloy Digest (1965) 14 (11): Ni-107.
Published: 01 November 1965
... MAR-M Alloy 200 is a nickel-base alloy designed primarily as a cast turbine blade material which retains useful strength up to 1900 F. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on high temperature...
Journal Articles
Alloy Digest (1964) 13 (2): Ni-88.
Published: 01 February 1964
... SM-200 is a nickel-base alloy designed primarily as a cast turbine blade material which retains useful strength up to 1900 F. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on high temperature performance as...
Journal Articles
Alloy Digest (1998) 47 (4): SS-711.
Published: 01 April 1998
... Carpenter type 204-Cu is a low-nickel, Manganese containing, austenitic stainless steel with copper. The copper provides a reduced work hardening rate for superior forming when compared to other 200 series stainless steels. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (2012) 61 (2): Fe-158.
Published: 01 February 2012
... SSC Invar 36 was developed for use in applications where dimensional stability is essential. It is a nickel-iron alloy with a very low coefficient of thermal expansion from cryogenic temperatures to 200 deg C (390 deg F). It is utilized in aerospace composite tooling and die applications, as well...
Journal Articles
Alloy Digest (1968) 17 (4): Ni-132.
Published: 01 April 1968
... lb. common salt, operating ac 180-1900F for 30-90 minutes immersion rime. After pickling, rinse in hoc water and neutralize in a l-2% volume ammonia solution. Specification Equivalents: ASTM F 290 General Characteri sties: This material differs from Nickel 200 in its higher manganese content which...