1-20 of 53 Search Results for

Nickel 211

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1968) 17 (4): Ni-132.
Published: 01 April 1968
... Nickel 211 is a nickel-manganese alloy recommended for improved resistance to attack by sulfur compounds at elevated temperatures. It is recommended for supports scaled in glass, grid wires in electron tubes, spark plug electrodes, etc. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1988) 37 (9): Ni-361.
Published: 01 September 1988
... CARPENTER NICKEL 211 ALLOY is a nickel-manganese alloy that is slightly harder than commercially pure nickel (Nickel 200). It is a solid-solution strengthened alloy. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information...
Journal Articles
Alloy Digest (1977) 26 (8): Ni-248.
Published: 01 August 1977
... TECHALLOY Nickel 211 is a nickel-manganese alloy with good elevated-temperature resistance to corrosion by sulfur compounds. When annealed, it is slightly stronger and harder than Techalloy Nickel 200 and is good for structural parts subjected to degassing temperatures. Nickel 211 has low electron...
Journal Articles
Alloy Digest (1972) 21 (1): SS-266.
Published: 01 January 1972
... ALLEGHENY TYPE 211 is a copper-bearing, austenitic, chromium-nickel-manganese stainless steel with a low work-hardening rate. It is used for many deep-drawing applications, such as automotive trim, and broiler pans, mixing bowls, sinks, and door hardware. This datasheet provides information...
Journal Articles
Alloy Digest (1974) 23 (11): Ni-211.
Published: 01 November 1974
... treatability joinability machinability physical properties tensile properties workability HASTELLOY Alloy C-4 Filing Code: Nickel Alloy Ni-211 NOVEMBER 1974 - DATA ON WORLD WIDE METALS AND ALLOYS HASTELLOY Alloy C-4 (Corrosion-Resistant High-Temperature Alloy) Pnblisbd by Engineering Alloys Digest...
Journal Articles
Alloy Digest (2011) 60 (9): Co-123.
Published: 01 September 2011
.... METGLAS® ALLOY 2714A (Magnetic Alloy) METGLAS® ALLOY 2714A Chemical Composition, wt Boron 1 5 Cobalt 75 90 Iron 7 13 Nickel 1 5 Silicon 7 13 Physical Properties: Density, kg/m3 (lb/in.3) 7590 (0.273) Lamination factor, % >75 Thermal expansion, 10 6/K (10 6/ºF) 12.7 (7.1) Crystallization temperature, ºC...
Journal Articles
Alloy Digest (2011) 60 (8): Co-122.
Published: 01 August 2011
... alloy designed for shielding and high frequency cores. METGLAS® ALLOY 2705M (Magnetic Alloy) METGLAS® ALLOY 2705M Chemical Composition, wt Boron 1 5 Cobalt 75 85 Iron 1 5 Molybdenum 1 5 Nickel 1 5 Silicon 3 7 Physical Properties: Density, kg/m3 (lb/in.3) 7800 (0.281) Lamination factor, % > 75 Thermal...
Journal Articles
Alloy Digest (1998) 47 (7): SS-723.
Published: 01 July 1998
... Allegheny Ludlum type 301 is the basic 18-8 chromium-nickel austenitic stainless steel with both chromium and nickel content lower than types 302 and 304. The steel is capable of attaining high tensile strength with good ductility by moderate or severe cold working. A typical application...
Journal Articles
Alloy Digest (1970) 19 (2): Cu-211.
Published: 01 February 1970
..., New Jersey PROMET 2s (Bearing Bronze) PROMET 2s is a highly leaded bronze recommended for bearings under boundary or mixed film conditions. Composition: Copper Tin Lead Nickel 70.0-75.0 4.0-5.5 19.0-23.0 0.20-0.8 Physical Constants: Density, Ib/cu. in. Electrical conductivity, WIACS Thermal coef...
Journal Articles
Alloy Digest (2006) 55 (7): Fe-139.
Published: 01 July 2006
... composition elasticity hardness heat treatability inductors METGLAS ALLOY 2605 SA1 physical properties tensile properties transformers workability thermal properties Chemical Composition, wt (Typical) Boron 1 5 Iron 85 95 Silicon 5 10 Cobalt (possible trace impurity) 0.2 max Nickel (possible race...
Journal Articles
Alloy Digest (1990) 39 (6): Cu-553.
Published: 01 June 1990
... Copper alloy No. C76390 is a wrought (rod) leaded nickel silver with nominally 24.5% nickel and 1% lead. This datasheet provides information on composition, physical properties, and elasticity. It also includes information on forming, heat treating, machining, and joining. Filing Code: Cu-553...
Journal Articles
Alloy Digest (2021) 70 (7): CS-211.
Published: 01 July 2021
... Molybdenum 0.045 0.40 0.70 0.40 0.70 Nickel 0.045 Copper 0.40 0.025 0.025 Iron 0.10 0.40 0.035 0.020 0.040 Heat Treatment 0.30 Transformation Temperatures 0.40 0.40 bal 0.10 0.10 Transformation temperature, in °C (°F) 0.40 0.40 Ac1 Ac3 Ms 730 (1346) 830 (1526) 420 (788) 0.30 0.30 bal bal Chromium...
Journal Articles
Alloy Digest (2012) 61 (4): SA-648.
Published: 01 April 2012
... Chemical Composition, wt (Typical Analysis) Carbon 0.20 Manganese 1.60 Phosphorus 0.025 Silicon 0.50 Sulfur 0.010 Chromium 1.00 Molybdenum 0.70 Nickel 1.50 Copper 0.40 Boron 0.004 Vanadium 0.10 Niobium 0.06 Iron bal Abrazo is offered with the following CEV: Maximum ladle CEV, thickness, mm...
Journal Articles
Alloy Digest (2005) 54 (5): Ni-625.
Published: 01 May 2005
... Haynes 617 is a solid-solution nickel-chromium-cobalt-molybdenum alloy with excellent high temperature strength and oxidation resistance. It has applications at high temperature for aerospace engines. This datasheet provides information on composition, physical properties, elasticity, and tensile...
Journal Articles
Alloy Digest (1974) 23 (11): Al-211.
Published: 01 November 1974
...: (Approximate) Copper 9.2-10.7 Density, lb/a in. Silicon 2.0 max. Specific gravtty Iron 1.5 max. Melting range, oF ZillC 0.8 max. Specific heat. cal/g/oC (At 1OOoC) Manganese 0.50 max. Thermal coef. expansion/OF (68-212oF) Nickel 0.50 max. (68-572oF) Magnesium 0.15-0.35 Thermal conductivity, cal/cm2/cm/seC...
Journal Articles
Alloy Digest (1988) 37 (10): CI-56.
Published: 01 October 1988
... carbon 3.00 max. Density, Ib/cu in. Silicon 1.75-3.00 Specific gravity Maw 0.7-1.00 Specific heat, Btu/lbPF Phosphorus 0.08 max. Melting point, F Nickel 18.00-22.00 Thermal coef. expansion/ F (704OOOF) Chromium 1.75-2.50 Thermal conductivity, Btu/ft*/in./h/ F (50-2OO F) Iron Remainder Electrical...
Journal Articles
Alloy Digest (1967) 16 (6): SA-211.
Published: 01 June 1967
... Sulphur Silicon Nickel Chromium Molybdenum Iron Physical Constants: 8720 8720H Density, lb cu.in. 0.283 0.18-0.23 0.1:-0.23 Melting point, F (approx.) 2760 0.70-0.90 0.60-0.95 Thermal conductivity, Btu; fr2inhr: F 260 0.035 max. Thermal coef. expansion, in. in: F x lo-6 0.040 max. 0.20-0.35 0.2010.35 0...
Journal Articles
Alloy Digest (1961) 10 (10): Ni-67.
Published: 01 October 1961
... CIRCLE LIN is a heat and corrosion resisting cast nickel-base alloy having high strength and resistance to oxidation at elevated temperatures. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness...
Journal Articles
Alloy Digest (2000) 49 (2): Ni-558.
Published: 01 February 2000
... on joining. Filing Code: Ni-558. Producer or source: Haynes International Inc. Producer or Source: Haynes International Inc. Copyright © ASM International® 2000 2000 ASM International bend strength chemical composition elasticity Haynes 230-W Filler Wire joinability nickel brazing filler...
Journal Articles
Alloy Digest (1990) 39 (6): Co-68.
Published: 01 June 1990
... JUNE 1990 - DIGEST- MAY 1974 DATA ON WORLD WIDE METALS AND ALLOYS CCc~y+t 1990. Alloy LT+st. Im. Allrights msented. Pkbhdby: Alby Digd. Inc. 1201.677.9161 Gatashownam~.nottok,dlbr 27 Canfdd SIreel. Orange. N.J. 07050 I U.S.A. MPI 59 ALLOY (High-Strength Nickel-Cobalt Base Alloy) MP159@ Alloy...