Alloy Digest (1990) 39 (5): Ni-383.
Published: 01 May 1990
... Carpenter Nickel 205 alloy exhibits an excellent combination of mechanical, electrical and corrosion resistant properties. It is resistant to oxidation. It is ferromagnetic below 680 F (360 C). The alloy is produced to closely controlled composition including small additions of magnesium...
Journal Articles
Alloy Digest (1964) 13 (3): Ni-89.
Published: 01 March 1964
... Nickel 205 is a nickel alloy having a high magnetostriction coefficient and is recommended for the electronic and electrical industries. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion...
Journal Articles
Alloy Digest (1977) 26 (7): Ni-247.
Published: 01 July 1977
... TECHALLOY Nickel 205 is a wrought nickel-base alloy containing small additions of magnesium and titanium. It has a high Curie temperature and a high magnetostriction coefficient. It is used for many electrical and electronic components and for equipment employing magnetostrictive effects...
Journal Articles
Alloy Digest (1994) 43 (9): Ni-464.
Published: 01 September 1994
...-205 ALLOY is an advanced corrosion resistant high-silicon alloy. Its major application is concentrated sulfuric acid. HASTELLDY and D-205 are trademarks of Haynes International, Inc. Composition, Wt, %: Nickel Chromium Iron Silicon Molybdenum Copper Carbon Nominal Bal. 20 6 5 2.5 2 0.03 max...
Journal Articles
Alloy Digest (1974) 23 (6): Ni-205.
Published: 01 June 1974
... heat resistance heat treatability joinability machinability physical properties powder metal products SPRAYWELD Process tensile properties wear resistance workability COLMONOY No. 62SA Filing Code: Ni-205 Nickel Alloy JUNE 1974 - DATA ON WORLD WIDE METALS AND ALLOYS Pvblisbed by Engineering...
Journal Articles
Alloy Digest (1968) 17 (4): Ni-132.
Published: 01 April 1968
... by barium, is lower than rhac of Nickel 205 making it useful for grid wires which may become contaminated with barium from the cathode. Availability: Nickel 211 is available in various forms as the product of a hear. Applications: Support wires, grid lateral winding wires, searchlight carbon holders...
Journal Articles
Alloy Digest (2020) 69 (4): Al-463.
Published: 01 April 2020
... Rio Tinto Alloy 242.2 is a heat-treatable, aluminum-copper-magnesium-nickel casting alloy. It is available in the form of ingots to be remelted for the manufacture of sand and permanent mold castings. Alloy 242.0 is used extensively for applications requiring high strength and hardness at elevated...
Journal Articles
Alloy Digest (1997) 46 (10): SS-640.
Published: 01 October 1997
... electrodes are not commercially made. How- ever, Type 205 is completely compatible with any weld metal used for the chromium-nickel austenitic stainless steels. The use of Type 310 covered electrodes will maintain the low magnetic permeability. Electrical resistance spof projection, and flash welding may...
Journal Articles
Alloy Digest (2020) 69 (3): TS-789.
Published: 01 March 2020
... Finkl Steel Durodi is a nickel-chromium-molybdenum-vanadium, alloy hot work tool steel that hardens deeply and uniformly to a high hardness that holds up exceedingly well under impact and thermal shock. It is designed to provide maximum abrasion and heat resistance over a full range of service...
Journal Articles
Alloy Digest (1986) 35 (4): Ni-332.
Published: 01 April 1986
... ELECTROLESS NICKEL is a nickel coating deposited by chemical reduction of nickel ions. The most widely used reducing agent is sodium hypophosphite. The thickness of the deposited coating is uniform over all areas of the work-piece that are in continuous contact with fresh plating solution...
Journal Articles
Alloy Digest (2010) 59 (12): Ni-684.
Published: 01 December 2010
... design. Published by: ASM International, Materials Park, OH 44073-0002, 440-338-5151 MemberServiceCenter@asminternational.org Fax 440-338-8542 www.asminternational.org Filing Code: Nickel December 2010 Ni-684 NAS 601 is Ni-Cr alloy with excellent oxidation resistance. The alloy is used extensively...
Journal Articles
Alloy Digest (1992) 41 (10): Ni-413.
Published: 01 October 1992
... BRUSH WELLMAN Alloy 360 beryllium nickel strip combines unique mechanical and physical properties required in electrical, electronic and electromechanical systems. Strength, stress-relaxation and fatigue are some of those properties. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1989) 38 (7): SS-509.
Published: 01 July 1989
... and nickel contents) with enhanced pitting and crevice corrosion resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining...
Journal Articles
Alloy Digest (1998) 47 (6): SS-721.
Published: 01 June 1998
...-bearing and high-nickel alloys. Its uniform corrosion resistance is better than type 304 in most media. Chloride pitting resistance is superior to type 316. Room temperature yield strength is nearly twice that of types 304 and 3 16. ln addition, Electrahoy Nitnmic 60 stainless steel provides excellent DOI...
Journal Articles
Alloy Digest (2016) 65 (11): SS-1255.
Published: 01 November 2016
... properties VDM NEUTROSHIELD workability thermal properties UNS S30460 to S30467 VDM NeutroShield is an austenitic stainless steel that is alloyed with boron to absorb neutrons. Chemical Composition, wt (Maximum) Chromium 0.08 Manganese 2.0 Silicon 0.75 Nickel 12 15 Chromium 18 20 Cobalt 0.2 Nitrogen...
Journal Articles
Alloy Digest (2012) 61 (10): Ni-702.
Published: 01 October 2012
... DMV 600L is a nickel alloy with 15.5 Cr. The alloy is used mainly as a material resistant to aqueous corrosion at temperatures below 450 deg C (842 deg F). This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information...
Journal Articles
Alloy Digest (2021) 70 (4): Ni-769.
Published: 01 April 2021
... VDM 601 (Nicrofer 6023 H) is a nickel-chromium-iron alloy with additions of aluminum and titanium. This alloy is specifically recommended for service above 550 °C (1020 °F) because of its superior creep-rupture properties resulting from its controlled carbon content and coarse grain size...
Journal Articles
Alloy Digest (1995) 44 (7): Ni-483.
Published: 01 July 1995
...-9161 27 Canlield SlreCn. Orange. N.J. 07060 I USA (Nickel-chromium-iron-alloy) SANDVIK SANICRO 70 is an austenitic alloy with good high temperature resistance to carburization and nitridation. The alloy is also very resistant to chloride-ion stress-corrosion cracking and to hydrogen chloride. SANICRO...
Journal Articles
Alloy Digest (1999) 48 (4): Ni-550.
Published: 01 April 1999
... joinability machinability physical properties tensile properties workability thermal properties UNS N10276 CARPENTER ALLOY C-276 (Nickel Alloy) Carpenter alloy C-276 is a Ni-Mo-Cr-W alloy with good fabricability. The alloy is balanced to provide excellent corrosion resistance to a vari- ety...
Journal Articles
Alloy Digest (2015) 64 (2): Ni-721.
Published: 01 February 2015
... DMV 600/600H are nickel alloys with 15.5 Cr. These stable, fully austenitic solid-solution alloys have higher carbon than alloy 600L (See Alloy Digest Ni-702, October 2012). This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well...