1-20 of 428 Search Results for

Ni-resist ductile iron

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1960) 9 (4): CI-28.
Published: 01 April 1960
... NI-RESIST DUCTILE IRONS are a group of austenitic nickel-alloyed cast irons having high strength and ductility combined with heat and corrosion resistance. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness...
Journal Articles
Alloy Digest (1996) 45 (2): Ni-499.
Published: 01 February 1996
... NI-ROD 55 Welding Electrode is used for shielded-metal-arc welding of gray, ductile, malleable, and Ni-Resist cast irons. It is also used for welding cast irons to various wrought materials, including carbon steels, low-alloy steels, and nickel alloys. The electrode is especially useful...
Journal Articles
Alloy Digest (1988) 37 (2): SS-493.
Published: 01 February 1988
... ARMCO A-286 is a precipitation-hardening austenitic Ni-Cr-Ti-Mo iron-base alloy that is especially useful for applications requiring high strength and oxidation resistance up to 1300 F (704 C). It has excellent notch-ductility. Its low magnetic permeability makes A-286 valuable where high strength...
Journal Articles
Alloy Digest (1989) 38 (1): Ni-366.
Published: 01 January 1989
... information on composition, physical properties, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-366. Producer or source: Allegheny Ludlum Corporation...
Journal Articles
Alloy Digest (1954) 3 (2): Ni-8.
Published: 01 February 1954
... REFRACTALOY 26 is a high heat resistant alloy of nickel, chromium, cobalt and iron, possessing high creep and endurance strengths along with high ductility at elevated temperatures. It responds to precipitation-hardening heat treatment. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1969) 18 (9): Ni-147.
Published: 01 September 1969
... information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on low and high temperature performance, and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ni-147...
Journal Articles
Alloy Digest (1995) 44 (11): Ni-490.
Published: 01 November 1995
... Electrode is supplied to AWS specifi- cations: AWS A5.15 Class ENi-Cl General Characteristics: NI-ROD Welding Electrodes are designed for general cast iron welding-joining gray iron, ductile iron, mal- leable iron, and alloy cast irons, including Ni-Resist and ductile Ni-Resist to themselves and to each...
Journal Articles
Alloy Digest (2003) 52 (10): Ni-615.
Published: 01 October 2003
... performance at elevated temperatures. The alloy is Ni-Fe-Mn with an addition of chromium and niobium to improve its resistance to high-temperature corrosion. This datasheet provides information on composition, hardness, and tensile properties. It also includes information on joining. Filing Code: Ni-615...
Journal Articles
Alloy Digest (1996) 45 (5): Ni-510.
Published: 01 May 1996
... graphite iron. malleable iron. and various alloyed irons such as Ni-Resist and Ductile Ni-Resists to themselves and to each other and to steels. stainless steels. and nickel alloys. Applications also include fabrication welding of cast-iron parts to other compo- nents. repair welding of broken or worn cast...
Journal Articles
Alloy Digest (1996) 45 (3): Ni-501.
Published: 01 March 1996
...-Resist and Ductile Ni-Resist to themselves and to each other and to steels, stainless steels, and nickel alloys. NI-ROD 99X Welding Electrode, with a core wire of commer- cially pure nickel, is recommended for welding thin cast-iron sections. Also, where optimum machinabihty of single-pass or single...
Journal Articles
Alloy Digest (2022) 71 (12): CI-100.
Published: 01 December 2022
... Typical microstructure in the center area (Etched in 5%Fig. 1 Typical microstructure in the center area (Etched in 5% Nital. 100×)Nital. 100×) CI-100 / 2 Comparable Grades Charter Dura-Bar Inc. EN 16482:2014 Dura-Bar 202 (Type 2) Ni-Resist iron General Characteristics Higher density than gray or ductile...
Journal Articles
Alloy Digest (1996) 45 (11): Fe-114.
Published: 01 November 1996
... in. diam wires. It can be used with all robotics. automatic, and semiautomatic processes and in all positions. NI-Rod Filler Metal 44 provides the wetting and crack- resistant weldability that allows steel forgings and castings to be automatically welded. Typical production-line applications would include...
Journal Articles
Alloy Digest (1995) 44 (5): Cu-600.
Published: 01 May 1995
... MAY 1995 DATA ON WORLD WIDE METALS AND ALLOYS CARLSON ALLOY 90 10 Cu Ni (Copper Nickel Alloy) 90-10 &pro-nickel is a highly ductile, malleable and corrosion resisting alloy, suitable for water applications. The alloy has approximately 1.4% iron to improve its &stance to sea water. It has good...
Journal Articles
Alloy Digest (1968) 17 (8): Fe-35.
Published: 01 August 1968
... or Source: Babcock & Wilcox Company Copyright © ASM International® 1996 1996 ASM International B & W IRON chemical composition corrosion-resistant alloys ductility elasticity electric motors generator housings hardness heat treatability joinability machinability magnetic...
Journal Articles
Alloy Digest (2001) 50 (6): Ni-569.
Published: 01 June 2001
... Equivalents: DIN EN 10027 Part 1, Material GX13NiCrNb37-25 General Characteristics: This alloy is an air melted iron-base alloy with low carbon con- tent, consisting essentially of a Fe-Ni-Cr matrix. The composition has been optimized to combine adequate high temperature strength and structural stability. Due...
Journal Articles
Alloy Digest (1986) 35 (3): CI-53.
Published: 01 March 1986
... and F34800. General Characteristics: AUSTEMPERED DUCTILE IRON (1.59i, Ni-0.39 MO) has strength comparable to heat-treated wrought steels. Itsstrength and ductility are as much as twice that of standard grades ofductile iron. Wear resistance. fatigue strength and fracture toughness are very good. Heat...
Journal Articles
Alloy Digest (1956) 5 (9): CI-16.
Published: 01 September 1956
... compromise between mechanical properties and oxidation resistance. Aurtdtzitic Type Highly alloyed ductile irons, produced and marketed as ductile Ni-Resist austenitic irons and containing 18- 30% Nickel and up w 5% cluomium, are available in several types which are especially useful for resistance...
Journal Articles
Alloy Digest (2008) 57 (7): Ni-664.
Published: 01 July 2008
... on corrosion resistance and surface qualities as well as heat treating and surface treatment. Filing Code: Ni-664. Producer or source: Wall Colmonoy Corporation. Producer or Source: Wall Colmonoy Corporation Copyright © ASM International® 2008 2008 ASM International abrasion resistance chemical...
Journal Articles
Alloy Digest (2001) 50 (8): Ni-571.
Published: 01 August 2001
... Kubota KHR45A LC is a modification of KHR45A (Alloy Digest Ni-570, July 2001) that changes either ductility or carburization resistance. The typical application is as outlet tubes and fittings in pyrolysis service. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1994) 43 (6): Ni-456.
Published: 01 June 1994
... corrosion-resistant alloys ductility elasticity electrical conductivity heat treatability joinability physical properties tensile properties thermal conductivity weldability workability wrought nickel alloys UNS N02200 N02201 CARLSON ALLOY C200 AND C201 Filing Code: Nickel Alloy Ni-456...