1-14 of 14 Search Results for

Ni-ROD WE

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1995) 44 (11): Ni-490.
Published: 01 November 1995
... or source: Inco Alloys International Inc. Producer or Source: Inco Alloys International Inc. Copyright © ASM International® 1996 1996 ASM International chemical composition ductility joinability Ni-ROD WE tensile properties welding electrodes UNS W82001 NI-ROD@WELDlNG FI FCTRODE ii Ni...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1972) 21 (7): Ni-176.
Published: 01 July 1972
... INCONEL alloy 600 (formerly INCONEL, Alloy Digest Ni-9, March 1954) is a nickel-chromium-iron alloy with good resistance to corrosion and heat. It is a solid-solution alloy that can be hardened only by cold working and it has excellent mechanical properties with a desirable combination of high...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1960) 9 (6): Cu-89.
Published: 01 June 1960
... spun, drawn, forged. Weldability: Best method gas shielded arc (either tungsten or metal). Good response to oxyacetylene welding, fair response to carbon arc welding, and welding. In carbon-arc we ding, zinc-free rods such p r response to resistance as copper-silicon or copper-tin are generally used...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1982) 31 (10): Ni-279.
Published: 01 October 1982
... BERYLCO Alloy 42C is a modification of BERYLCO Alloy 41C (Alloy Digest Ni-251, November 1977). Alloy 42C is a highly castable, air-melting, nickel-base alloy that can be precipitation hardened (aged) to high strength and hardness. It is a stainless alloy and exhibits excellent resistance to wear...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1955) 4 (7): CI-11.
Published: 01 July 1955
... or 6ller rods of Monel, nickel or Ni-Resist, so that the weid metal will have sitrdar corrosioo proper& ro the Ni-Resist co be welded. In merallic-arc welding use Monel 130x elecoodc Reheat to ZOO-lOOO F, and afrer welding, the entire casting should be permiaed co cool slowly from the we =P=a== Corrosion...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1996) 45 (11): Ni-518.
Published: 01 November 1996
..., elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-518. Producer or source: VDM Technologies Corporation. Producer or Source: VDM Technologies Corporation Copyright © ASM International® 1996...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1953) 2 (5): Ni-4.
Published: 01 May 1953
..., physical properties, hardness, and tensile properties as well as creep. It also includes information on forming, machining, and joining. Filing Code: Ni-4. Producer or source: International Nickel Company Inc.. Producer or Source: International Nickel Company Inc. Copyright © ASM International® 1996...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1995) 44 (11): Ni-491.
Published: 01 November 1995
... country National StUKiard Germany DIN UnitedKingdom USA ASTM specificlllion chQn. Tube and pipe Sheet Rod s* Wire Forgings Material -PO- and and designation sition seamIess welded Plate bar W.-Nr. 2.4066 Ni 99.2 17740 17751 17751 17750 17752 17750 in53 17754 NA 11 3074 3072 3076 3073 3075 UNSNO2200 B 161...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1956) 5 (12): Ni-30.
Published: 01 December 1956
... toughness and creep. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-30. Producer or source: Haynes Stellite Company. Producer or Source: Haynes Stellite Company Copyright © ASM International® 1996 1996 ASM International...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1971) 20 (10): Ni-5.
Published: 01 October 1971
..., and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-5. Producer or source: Carpenter Technology Corporation. Originally published May 1953, revised October 1971. Producer...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1977) 26 (11): Ni-251.
Published: 01 November 1977
... BERYLCO Alloy 41C is a highly castable, air-melting nickel-base alloy; it is precipitation-hardenable to high strength and hardness. It exhibits excellent resistance to wear, corrosion and oxidation. Alloy 41C (formerly called Berylco CR-1, Alloy Digest Ni-27, September 1956) is the standard...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1953) 2 (3): Ni-3.
Published: 01 March 1953
... properties, hardness, elasticity, and tensile properties as well as fracture toughness, creep, and fatigue. It also includes information on high temperature performance as well as heat treating, machining, joining, and surface treatment. Filing Code: Ni-3. Producer or source: International Nickel Company Inc...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1998) 47 (3): In-3.
Published: 01 March 1998
.... High purity indium is used in electronic device technology. crystal growth in epitaxial processes, and the production of single crystal I&V compound semiconductors. Chemical Composition: ~-P==paW(ppbh) 6N 6Ns 6Nswa 7N B Al w Si S Fe Ni ch zm Ga E cd sn n Pb Bi MO ca Toral-ilD- Cl00 60 Cl00 Cl0 ND 40...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1965) 14 (11): SS-174.
Published: 01 November 1965
... by we&. After pickling, rinse thoroughly and dip in a warm solu- tion of 15.30% nitric acid by weight, and wash In water. Workability: TO forge, heat slowly to 1800 deg. F and soak at this temperature a sufficient length of time, then raise temperature CO 2100.2250 deg. F. Forging can be continued...