Alloy Digest (1963) 12 (1): Cu-124.
Published: 01 January 1963
... Ni-Bral nickel-aluminum bronze is a material having high strength and good corrosion resistance. It is recommended for marine propellers, impellers, valves, gears, and shafting. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties...