Journal Articles
Alloy Digest (1976) 25 (11): Ni-236.
Published: 01 November 1976
... NUCALLOY 41 is a nickel-chromium-boron alloy developed as an alternative to cobalt-base alloys in applications where the presence of cobalt is undesirable. It is finding wide acceptance because of its toughness and high resistance to attack by many chemicals. It has superior wear resistance which...
Journal Articles
Alloy Digest (1997) 46 (6): Ni-528.
Published: 01 June 1997
... NUCALLOY ALLOYS 453 and 488 are nickel-base hardfacing alloys designed to replace the traditional cobalt alloys for nuclear plant applications. These alloys have been used in Japanese commercial nuclear power plant service. This datasheet provides information on composition, physical properties...