Alloy Digest (2015) 64 (8): SS-1221.
Published: 01 August 2015
... NSSMC NAR-305G is a nonmagnetic austenitic stainless steel even when cold worked. This datasheet provides information on composition, hardness, and tensile properties. It also includes information on forming. Filing Code: SS-1221. Producer or source: Nippon Steel and Sumitomo Metal Corporation...