Alloy Digest (2019) 68 (10): SS-1310.
Published: 01 October 2019
... NSSMC Advanced 347AP is an austenitic stainless steel with excellent polythionic acid resistance and good high-temperature strength. This datasheet provides information on composition as well as creep. It also includes information on high temperature performance. Filing Code: SS-1310. Producer...