Alloy Digest (2011) 60 (12): SS-1111.
Published: 01 December 2011
... NSSC FW1 is one of the first ferritic stainless steels to have tin (Sn) added as a specific alloying element and is one alloy of an FW series. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information...