Alloy Digest (1997) 46 (10): Fe-115.
Published: 01 October 1997
... Novalloy 280 is a nickel-cobalt steel fastener alloy that was introduced for use in military and aerospace applications, but now is available for general fastener use. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well...