1-1 of 1 Search Results for

NOREM 02

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1994) 43 (12): SS-576.
Published: 01 December 1994
... NOREM 02 is a welding consumable for use in nuclear power plant systems to be part of the cobalt reduction program by EPRI to control radiation fields. The alloy can be used for hardfacing in valves with good results. This datasheet provides information on composition. It also includes information...