1-17 of 17 Search Results for

NITRONIC 20

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1981) 30 (2): SS-381.
Published: 01 February 1981
... Nitronic 20 was designed for elevated-temperature use where high mechanical strength and resistance to oxidation and sulfidation are important. This stainless steel exhibits high mechanical strength throughout the 1000-1700 F (538-927 C) temperature range, yet it is malleable at forging...
Journal Articles
Alloy Digest (1976) 25 (1): SS-324.
Published: 01 January 1976
... 94000 63 -100 166000 1040@0 60 -150 179000 1 16000 55 -200 195000 132000 50 -242 108000 146000 42 -320 33000 175000 20 Copyright © ASM International® 1996DOI: 10.31399/asm.ad.ss0324 Table 7 - TYPICAL LOW-TEMPERATURE TOUGHNESS OF NITRONIC 33 AND AISI TYPE 304 Yield Strength Notch Strength Ratio Notched...
Journal Articles
Alloy Digest (2005) 54 (6): SS-931.
Published: 01 June 2005
... Carlson alloy Nitronic 33 has twice the yield strength of 304 stainless with comparable corrosion resistance. The low magnetic permeability of the alloy is retained after severe cold working. The resistance to chloride stress-corrosion cracking is superior to Type 304. Nitronic 33 has excellent...
Journal Articles
Alloy Digest (2013) 62 (4): SS-1142.
Published: 01 April 2013
... Electralloy’s Nitronic 33 is a nitrogen strengthened austenitic stainless steel. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on corrosion and wear resistance as well as forming, heat treating, machining, and joining...
Journal Articles
Alloy Digest (1975) 24 (11): SS-320.
Published: 01 November 1975
... NITRONIC 32 is basically a low-nickel chromium-manganese austenitic stainless steel strengthened by an addition of nitrogen. It has annealed strength approximately two times that of AISI Type 304 stainless steel and comparable corrosion resistance. It is used in such applications as fasteners...
Journal Articles
Alloy Digest (2018) 67 (9): SS-1294.
Published: 01 September 2018
... Electralloy Nitronic 32 was created to match AISI Type 304 Stainless Steel in corrosion with twice the yield strength. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on corrosion resistance as well as joining. Filing...
Journal Articles
Alloy Digest (1998) 47 (5): SS-715.
Published: 01 May 1998
... Electralloy Nitronic 50 provides a combination of corrosion-resistance wear and strength not found in other stainless steels. High-speed (HS) Nitronic 50 has a yield strength that is 3 to 4 times that of type 316 stainless steel. This datasheet provides information on composition and physical...
Journal Articles
Alloy Digest (1992) 41 (8): SS-533.
Published: 01 August 1992
... NITRONIC 30 is a nitrogen-strengthened stainless steel with a good combination of strength, corrosion and wet abrasive wear resistance and economy. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness...
Journal Articles
Alloy Digest (1998) 47 (6): SS-721.
Published: 01 June 1998
... Electralloy Nitronic 60 is an alloy with excellent uniform corrosion resistance, outstanding galling resistance, high strength, and good high-temperature oxidation resistance. The alloy retains toughness at low temperature. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (2008) 57 (12): SS-1025.
Published: 01 December 2008
... Carlson Alloy Nitronic 50 has corrosion resistance superior to 316L and 317L with twice the yield strength at ambient temperatures. It possesses good mechanical properties at both elevated and subzero temperatures, and retains low magnetic permeability even after severe cold working or at subzero...
Journal Articles
Alloy Digest (2013) 62 (3): SS-1138.
Published: 01 March 2013
... AK Steel Nitronic 30 has good wet abrasion resistance, good resistance to aqueous and atmospheric corrosion, high strength, economy, and improved stress-corrosion cracking resistance over common 18-8 stainless steels. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (2018) 67 (10): SS-1295.
Published: 01 October 2018
... (Btu/(h·ft·ºF)) 20 ºC (68 ºF) 12.0 (6.9) 100 °C (212 °F) 15.9 (9.2) Copyright © 2018, ASM International®. All rights reserved. ELECTRALLOY ALLOY NITRONIC 33 (Low Nickel Austenitic Stainless Steel) Filing Code: SS-1295 Stainless Steel :: October 2018 Materials Park, Ohio 44073-0002 :: 440.338.5151...
Journal Articles
Alloy Digest (2014) 63 (2): SS-1168.
Published: 01 February 2014
... values, 20 100 °C (68 212 °F), 10 6/K (10 6/°F) 15 (8) Modulus of elasticity, 20 °C (68 °F), GPa (106 psi) 195 (28) Mechanical Properties: Tensile Strength. This alloy is tested and certified according to minimum breaking load specified in the dimensional table. See Table 1. Proof Strength. Rp0.2...
Journal Articles
Alloy Digest (2002) 51 (1): SS-841.
Published: 01 January 2002
... Alloy 19D (UNS S32001), Nitronic 19D, is a lean duplex (ferritic-austenitic) stainless steel developed by AK Steel. Compared to conventional duplex and super-duplex stainless steels, alloy 19D has a reduced chromium content, man-ganese is substituted for most of the nickel, and molybdenum...
Journal Articles
Alloy Digest (1977) 26 (4): SS-338.
Published: 01 April 1977
...) 5000~517) 60000 (414) ssooo 079) Torsion. min 5OOOGl345) 70000 (483) 50000 (345) 40000 (276) 36600 (252) Elongatwn i2 III min ? Reducuon aI area. mm: r, 20 20 25 30 30 50 50 50 SO 50 Charpy impact (V-march). it.lbf II Typical values lOO+ (136*) lOO(l36! lOO+tl36+j IOP (136+) IOP (136+) *MPa...
Journal Articles
Alloy Digest (2021) 70 (6): SS-1336.
Published: 01 June 2021
... Rp0.2 A(a) 20 100 °C % Coefficient of linear 10 6/K (68 212 °F) 10.5 MPa ksi MPa ksi 20 thermal expansion (10 6/°F) 20 300 °C (5.8)(a) 30 (32 600 °F) Specification 415 60 276 40 11.5 Typical values(b) 20 °C (6.4)(a) 476 69 379 55 (68 °F) Thermal W/(m K) 20 °C 30 Rp0.2 = 0.2% proof strength; Rm...
Journal Articles
Alloy Digest (1976) 25 (8): SS-332.
Published: 01 August 1976
... tools Milling (end mill Super H-S steel tools Threading. die head, H-S steel tools Threading, single point, H-S steel tools Carbide tools Drilling, High-Speed steel tools Saw Cutting (Heavy Pressure) Reciprocating H-S steel blade Band saw Speed sfpm Feed IO01SO 0.005-0.015 in./rev 130-l 20 0.003-0.005...