Skip Nav Destination
Close Modal
Search Results for
NIROSTA 4561
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-1 of 1
Search Results for NIROSTA 4561
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
NIROSTA 4561: Austenitic Stainless Steel
Available to Purchase
Alloy Digest (2005) 54 (10): SS-943.
Published: 01 October 2005
... Nirosta 4561 is a very-low-carbon, stabilized with titanium, version of the molybdenum-containing corrosion-resistant austenitic stainless steels. The alloy resists exhaust gases and is used in flues. This datasheet provides information on composition, physical properties, elasticity, and tensile...
Abstract
View articletitled, <span class="search-highlight">NIROSTA</span> <span class="search-highlight">4561</span>: Austenitic Stainless Steel
View
PDF
for article titled, <span class="search-highlight">NIROSTA</span> <span class="search-highlight">4561</span>: Austenitic Stainless Steel
Nirosta 4561 is a very-low-carbon, stabilized with titanium, version of the molybdenum-containing corrosion-resistant austenitic stainless steels. The alloy resists exhaust gases and is used in flues. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-943. Producer or source: ThyssenKrupp Nirosta GmbH.