Alloy Digest (2002) 51 (10): SS-864.
Published: 01 October 2002
... Nirosta 4315 is an austenitic stainless steel of the 18Cr-10Ni-type strengthened with nitrogen. The alloy possesses much the same corrosion resistance as Type 304, but maintains higher strength and toughness. This datasheet provides information on composition, physical properties, elasticity...