Journal Articles
Alloy Digest (2002) 51 (3): Ni-581.
Published: 01 March 2002
... Nimrod 625 and 625KS are Inconel-type consumables with molybdenum and niobium. They are used to join UNS N06625 and Nicrofer 6020hMo of similar composition and also for other lower alloys to ensure the weld has as good or better corrosion resistance as does the base metal. This datasheet provides...
Journal Articles
Alloy Digest (2003) 52 (1): Ni-599.
Published: 01 January 2003
..., this consumable is suitable for welding heat-resistant alloys including Inconel 601 (except in severe sulfidizing condi- tions), Incoloy 800/800H (preferred to Nimrod AKS above about 900 °C, or 1652 °F) or combinations of these with other alloys for furnace equipment, petrochemical, and power- generation plants...
Journal Articles
Alloy Digest (2002) 51 (7): Ni-588.
Published: 01 July 2002
... Nimrod C22KS is a nickel-chromium-molybdenum-tungsten type consumable with a nominal composition of Ni, 22% Cr, 13.5% Mo, and 3% W and is used to join high-molybdenum corrosion-resistant alloys to themselves and each other. This datasheet provides information on composition, hardness, and tensile...
Journal Articles
Alloy Digest (2002) 51 (12): Ni-596.
Published: 01 December 2002
... Nimrod 59KS is a basic all-positional pipe-welding electrode for Alloy 59 (see NICROFER 5923 hMo, Alloy Digest Ni-430, May 1993) and other highly corrosion-resistant alloys with very high molybdenum content. This datasheet provides information on composition and tensile properties as well...
Journal Articles
Alloy Digest (2002) 51 (8): Ni-589.
Published: 01 August 2002
... NimRod C276 and C276KS are Ni-Cr-Mo-W-type welding consumables with a nominal composition of Ni, 15% Cr, 16% Mo, 4% W, and 5% Fe. They are used to join high-molybdenum-containing corrosion-resistant alloys to themselves and each other. This datasheet provides information on composition, hardness...