Alloy Digest (2002) 51 (2): Ni-578.
Published: 01 February 2002
... Nimrod 182 and 182KS are Inconel-type consumables containing manganese and niobium. The electrodes are used to join nickel-base alloys to themselves and to mild, low-alloy, and stainless steels. These weld metals are also used for transition joints and with cryogenic 3 and 5% Ni steels...
Journal Articles
Alloy Digest (2003) 52 (3): Ni-603.
Published: 01 March 2003
... Metrode Nimrod AKS and AB, and Nimax A are nickel-base consumables similar to 182, but with lower manganese and with a molybdenum addition. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness. It also includes information on joining...
Journal Articles
Alloy Digest (2003) 52 (5): Ni-607.
Published: 01 May 2003
... Metrode Nimrod 132KS is a nickel-base consumable with uses similar to 182 and Metrode 20.70Nb. The nominal composition is 70Ni-16.5Cr-6.5Fe and 2.5 Nb. This datasheet provides information on composition and tensile properties as well as fracture toughness. It also includes information on joining...