Alloy Digest (1987) 36 (7): Ni-350.
Published: 01 July 1987
... NIMONIC Alloy 263 is an air-melted nickel-base alloy which has improved ductility in welded assembly. Developed originally as a sheet material, it is available in all standard forms. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2003) 52 (9): Ni-613.
Published: 01 September 2003
... (1400 ┬░F). Maximum hardness is attained in 12 h. Fabricability: Alloy 740 is readily fabricated in the annealed condition. Weldability: Joining is accomplished with the gas tungsten arc welding (GTAW) process using Nimonic Filler Metal 263. If a high joint strength is required, the deposited weldment...