Alloy Digest (1976) 25 (10): Ni-234.
Published: 01 October 1976
... NIMAG 101 combines good mechanical properties with good corrosion resistance. It retains its strength to a high degree at elevated temperatures. Close control of composition is achieved by vacuum melting. This material has a wide range of electrical and electronic applications. Nimag 101 is a low...