Alloy Digest (1976) 25 (3): Ni-224.
Published: 01 March 1976
... NIMAG 100 is wrought nickel combining excellent mechanical properties with good corrosion resistance. It retains its strength to a high degree at elevated temperatures. Nimag 100 is produced by vacuum melting to provide close control of composition. It is used in a wide range of electrical and...
Journal Articles
Alloy Digest (1976) 25 (10): Ni-234.
Published: 01 October 1976
...-carbon version of Nimag 100. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface...
Journal Articles
Alloy Digest (1976) 25 (8): Ni-231.
Published: 01 August 1976
... Nimag 100. The strength and base hardness of Nimag 111 when fully annealed are slightly greater than those of Nimag 100. Structural parts made of Nimag 11 1 retain strength when subject to degassing temperatures. Forms Available: Plate, strip, foil and cut flat sheets. Applications: Electron tubes and...
Journal Articles
Alloy Digest (1977) 26 (2): Ni-240.
Published: 01 February 1977
... NIMAG 60 is a non-magnetic nickel alloy with good resistance to oxidation at high temperatures and to corrosion in many environments. It is a solid-solution alloy that can be hardened only by cold working and it has excellent mechanical properties with a desirable combination of high strength and...