Alloy Digest (1995) 44 (10): Ni-488.
Published: 01 October 1995
... NILOMAG ALLOY 77 is a 77 Ni soft magnetic alloy with a high level of initial permeability. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on heat treating. Filing Code: Ni-488. Producer or source: Inco Alloys...