... NILO alloy 475 is an iron-nickel-chromium glass-sealing alloy. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Fe...