Alloy Digest (1987) 36 (6): Fe-77.
Published: 01 June 1987
... NILO Alloy 42 is a binary nickel-iron alloy having a low and nominally constant expansion coefficient over the range 20-300 C (68-572 F). It is used for semiconductor lead frames, thermostats and glass-to-metal seals. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1987) 36 (8): Fe-79.
Published: 01 August 1987
... NILO alloy 36 is a binary iron-nickel alloy having a very low and essentially constant coefficient of thermal expansion at atmospheric temperatures. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on high...