Alloy Digest (1959) 8 (12): TS-87.
Published: 01 December 1959
... NIKRO-M is a tough, deep-hardening tool steel suitable for general purpose shock resisting applications. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness, and deformation. It also includes information on forming, heat treating...
Journal Articles
Alloy Digest (1971) 20 (1): TS-232.
Published: 01 January 1971
...: Bethaloy Bethlehem Tioga Allegheny Ludlum RDS Carpenter Nicrodie Columbia Champaloy Crucible ET-4 Jessop NDS Latrobe Cyclops L6 Universal-Cyclops Nikro M Vasco General Characteristics: AlSl Type L6 is a family of high-carbon low-alloy tool steels designed to provide oil-hardening capabilities and higher...
Journal Articles
Alloy Digest (2018) 67 (5): Fe-168.
Published: 01 May 2018
...) Thermal conductivity, 20 80 °C (68 176 °F), W/m·K (Btu/(h·ft·°F)) 17.1 (9.9) Electrical resistivity, 20 °C (68 °F), m ( circular- mil/ft) 0.806 (485) Copyright © 2018, ASM International®. All rights reserved. Ferro-Titanit® Nikro 143 (Carbide Alloyed Iron-Nickel-Cobalt Alloy) Filing Code: Fe-168 Iron...
Journal Articles
Alloy Digest (2018) 67 (4): SS-1283.
Published: 01 April 2018
... Ferro-Titanit Nikro 128 is one of a series of metal-matrix composites manufactured by a powder metallurgy process and is a range of carbide-alloyed materials from Deutsche Edelstahlwerke. The matrix structure consists of a highly tough, age-hardenable nickel martensite. The chromium content...
Journal Articles
Alloy Digest (2018) 67 (6): SS-1290.
Published: 01 June 2018
..., 22300 Hz 18 Thermal conductivity, 20 °C (68 °F), W/m·K (Btu/ (h·ft·°F)) 18.8 (10.9) Electrical resistivity, 20 °C (68 °F), m ( circular-mil/ft) 0.77 (463) Magnetic Properties Magnetic saturation polarization, T (G) 0.62 (6200) Coercive field strength, A/m (Oe) 9800 (123) Remanence, T (G) 0.108 (1080...
Journal Articles
Alloy Digest (2018) 67 (2): SA-812.
Published: 01 February 2018
... (68 572 °F) 9.8 (5.44) Thermal conductivity, 20 °C (68 °F), W/m·K (Btu/(h·ft·°F)) 20.5 (11.8) Damping Q 1 (10 5) Measuring frequency, 2000 Hz 14 Measuring frequency, 7000 Hz 22 Measuring frequency, 22000 Hz 16 Electrical resistivity, 20 °C (68 °F), m ( circular-mil/ft) 0.75 (451) Magnetic Properties...