Alloy Digest (1992) 41 (1): Ni-400.
Published: 01 January 1992
... TOPHEL Alloy and NIAL Alloy are respectively the positive and negative thermoelements for ISA Type K thermocouples. NICROSIL/NISIL Alloys are respectively the positive and negative thermoelements of ISA Type N thermocouples. Thermocouples of 20 and 19 Alloys have the advantage of freedom from...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2012) 61 (2): Cu-803.
Published: 01 February 2012
... (15.5) NICROSIL + 100 (+ 56) 13.3 (7.4) 13.0 (7.5) NISIL + 900 (+ 500) 12.1 (6.7) 23.0 (13.3) PCLW-SNX + 2100 (+ 1167) 21.0 (12.1) PCLW-8PX + 3700 (+ 2056) 71 (41) 19 Alloy + 3050 (+ 1694) 13.6 (7.6) 50 (29) 20 Alloy + 290 (+ 161) 11.9 (6.6) 13 (8) DOI: 10.31399/asm.ad.cu0803 Fig. 1 EMF curves...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2015) 64 (10): Cu-842.
Published: 01 October 2015
... mechanical properties thermocouple alloys Alloy Yield strength, 20 ºC (68 ºF), MPa (ksi) Tensile strength, 20 ºC (68 ºF), MPa (ksi) Elongation, 8 gage, 20 ºC (68 ºF), % Cupron 345 (50) 586 (85) 45 Tophel 207 (30) 608 (88) 45 Nial 193 (28) 572 (83) 45 Nicrosil 414 (60) 758 (110) 30 Nisil 379 (55) 655 (95...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2019) 68 (5): Ni-751.
Published: 01 May 2019
... strength, 20 °C (68 °F), MPa (ksi) Tensile strength, 20 °C (68 °F), MPa (ksi) Elongation, 20 °C (68 °F), 8 gage, % Cupron 345 (50) 586 (85) 45 Tophel 207 (30) 607 (88) 45 NIAL 28 (193) 572 (83) 45 Nicrosil 414 (60) 758 (110) 30 Nisil 379 (55) 655 (95) 35 PCLW-SNX 124 (18) 262 (38) 20 PCLW-8PX 103 (15) 276...