Alloy Digest (2003) 52 (10): Ni-616.
Published: 01 October 2003
... Nicrofer 5020 hMo (also known as 50 PLUS) is a low-carbon Ni-Cr-Fe-Mo alloy with excellent wet corrosion resistance. The alloy has versatility in use as a wrought alloy or filler metal for lower-alloy materials such as 6–7% Mo stainless steels. This datasheet provides information on composition...