Alloy Digest (1985) 34 (7): Ni-318.
Published: 01 July 1985
... NICROFER 4823 HMo is an austenitic nickel-chromium-iron alloy with increased molybdenum and an addition of copper. The alloy has very good corrosion resistance to a wide range of corrosive media under both oxidizing and reducing conditions. It also has excellent resistance to crevice corrosion...