Alloy Digest (1988) 37 (7): Ni-358.
Published: 01 July 1988
... NICROFER 4722 Co is a high-strength matrix-stiffened nickel-chromium-molybdenum-iron alloy with cobalt and tungsten additions. It has excellent oxidation resistance up to 2190 F (1200 C). This datasheet provides information on composition, physical properties, elasticity, and tensile properties...