Alloy Digest (1994) 43 (12): Ni-472.
Published: 01 December 1994
... NICROBRAZ 160 is for wide clearance joints where heavier fillets or greater joint ductility and machinability are desired. This datasheet provides information on composition, physical properties, and hardness. It also includes information on corrosion resistance as well as joining. Filing Code: Ni...
Journal Articles
Alloy Digest (1997) 46 (2): Ni-522.
Published: 01 February 1997
... Nicrobraz 110 is a low-melting brazing filler metal with improved corrosion resistance for applications requiring high joint strength and oxidation resistance up to 2200F. This datasheet provides information on composition, physical properties, and hardness. It also includes information...
Journal Articles
Alloy Digest (1994) 43 (5): Ni-452.
Published: 01 May 1994
... NICROBRAZ LM is a low melting general-purpose brazing filter metal for applications requiring high joint strength and oxidation resistance up to 2200 F. This datasheet provides information on composition and physical properties. It also includes information on corrosion resistance as well...