Skip Nav Destination
Close Modal
Search Results for
NICOMET 2
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-2 of 2 Search Results for
NICOMET 2
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2000) 49 (9): Cu-653.
Published: 01 September 2000
... Nicomet 2 is a copper-nickel-tin alloy that has high strength because of spinodal decomposition. The alloy has good antifriction properties. Nicomet 2 could replace some beryllium-copper alloys. An example application for the alloy is a sleeve bearing. This datasheet provides information...
Abstract
View article
PDF
Nicomet 2 is a copper-nickel-tin alloy that has high strength because of spinodal decomposition. The alloy has good antifriction properties. Nicomet 2 could replace some beryllium-copper alloys. An example application for the alloy is a sleeve bearing. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on wear resistance as well as heat treating. Filing Code: CU-653. Producer or source: Anchor Bronze & Metals, Inc.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2000) 49 (8): Cu-652.
Published: 01 August 2000
... treatment. The alloy could replace alu- minum and manganese bronzes. A typical application utilizes both the good antifriction and high strength properties. Nicomet is a registered trademark of Anchor Bronze and Metals, Inc. Chemical Composition, wt (Nominal) Copper 88 Tin 5 Nickel 5 Zinc 2 Other elements...
Abstract
View article
PDF
Nicomet 1 is a copper-nickel-tin alloy that has high strength because of spinodal decomposition in heat treatment. The alloy could replace aluminum and manganese bronzes. A typical application utilizes both the good antifriction and high strength properties. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on wear resistance as well as heat treating. Filing Code: CU-652. Producer or source: Anchor Bronze & Metals, Inc.