Skip Nav Destination
Close Modal
Search Results for
NICKELVAC H-X
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-3 of 3 Search Results for
NICKELVAC H-X
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1990) 39 (4): Ni-381.
Published: 01 April 1990
... ASM International chemical composition corrosion-resistant alloys creep properties elasticity heat treatability high-temperature alloys joinability low-temperature alloys machinability NICKELVAC H-X oxidation resistance physical properties tensile properties weldability workability...
Abstract
View article
PDF
NICKEL VAC H-X is a non-heatreatable nickel-base alloy with excellent cold forming and welding characteristics. It has good strength and oxidation resistance up to 2200 F(1204 C). This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on low and high temperature performance, and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-381. Producer or source: Teledyne Allvac.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1990) 39 (11): Ni-387.
Published: 01 November 1990
...: 10.31399/asm.ad.ni0387 Copyright © ASM International® 1996 100 60 - 20 9 2 10 k! $5 1 NEAT TREATMENTS 2lSO.F -1 Mr. AIR COOL 690 1 5 10 TIME-H& 100 500 1000 FIGURE 3 - Stress-rupture life of NICKELVAC X-751 in the range 1 350-1700°F(732-927 Heat Treatment: Solution treatmenu 2150°F(11770C)/1 hr.,aircool...
Abstract
View article
PDF
NICKEL VAC X-751 is a modification of NICKEL VAC X-750 carrying higher aluminum content (0.90-1.50 vs 0.4-1.0%). This raises the maximum service temperature 100 F(55 C) to 1600 F(871 C). NICKEL VAC X-751 has a simplified and shortened heat treating cycle relative to NICKEL VAC X-750. It is produced by vacuum induction melting followed by vacuum arc or electroslag remelting. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-387. Producer or source: Teledyne Allvac.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1965) 14 (2): Ni-98.
Published: 01 February 1965
... Nickelvac Super-X is a nickel-base alloy recommended for applications requiring oxidation and corrosion resistance coupled with good strength up to 1200-1500 F. It is used in gas turbines heat engines, high temperature bolts and forming tools. This datasheet provides information on composition...
Abstract
View article
PDF
Nickelvac Super-X is a nickel-base alloy recommended for applications requiring oxidation and corrosion resistance coupled with good strength up to 1200-1500 F. It is used in gas turbines heat engines, high temperature bolts and forming tools. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ni-98. Producer or source: Allvac Metals Company.