Alloy Digest (1985) 34 (1): Ni-308.
Published: 01 January 1985
... Nickel Filler Metal 61 is a nickel-base alloy that is used for welding Nickel 200 and Nickel 201 to themselves and to other alloys such as stainless steel, carbon steels, copper-nickel alloys, INCONEL alloys, INCOLOY alloys and MONEL alloys. The weld metal has moderate strength and ductility...
Journal Articles
Alloy Digest (1985) 34 (9): Ni-321.
Published: 01 September 1985
... for surfacing of steel; gas-metal-arc surfacing should be done only after a barrier layer of Nickel Filler Metal 61 is applied. Submerged-arc welding with Filler Metal 60 is done with INCO-FLUX 5 Submerged Arc Flux. A barrier layer is not needed for submerged-arc surfacing. Weld metal deposited by Filler Metal...
Journal Articles
Alloy Digest (2011) 60 (2): Ni-686.
Published: 01 February 2011
...) Mechanical Properties: Typical mechanical properties are shown in Table 1. Weldability: Nickel 270 has been welded successfully by the shielded metal- arc process using nickel welding electrode 141 and by the gas- tungsten-arc process using nickel filler metal 61. In resistance welding, a high current...
Journal Articles
Alloy Digest (1968) 17 (4): Ni-132.
Published: 01 April 1968
... not to hear rhe metal above the upper limits. Tallow, soap, soluble oil and similar heavy lubricants are used in connection with cold-working operations. Weldability: Nickel 211 may be welded by the oxyacetylene process using Nickel Filler Metal 41, the gas-shielded arc processes using Nickel Filler Metal 61...
Journal Articles
Alloy Digest (1963) 12 (6): Ni-83.
Published: 01 June 1963
... for metallic arc welding and No. 61 filler rod for inert-gas metal-arc welding. The recomm ended welding process is tungsten arc inert gas shielded, using Nickel Filler Metal 61. Welds should be aged w develop maximum saengrh but aging response will not be as great as that of rhe base metal. Welding shwld...
Journal Articles
Alloy Digest (1969) 18 (3): Ni-143.
Published: 01 March 1969
... Nickel 270 is a high purity nickel exceptionally free from non-metallic inclusions. Its low hardness and good ductility permit heavy cold deformation without reannealing. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also...
Journal Articles
Alloy Digest (1968) 17 (9): Ni-138.
Published: 01 September 1968
... Filler Metal 61 or equivalent. Corrosion Resistance: Very high resistance to all kinds of corrosive media except a sulphurous condition. Will resist alkalis, mineral acids and organic acids, but not oxidizing acids or oxidizing salts. Nitric acid readily attacks the alloy. OXIDATION RESISTANCE (Exposure...
Journal Articles
Alloy Digest (1969) 18 (2): Ni-142.
Published: 01 February 1969
... or other materials use Into Weld-A electrode or equivalent. For inert-gas arc welding of the alloy to itself use Into Nickel Filler Metal 61 or equivalent. Beryllium combines with nickel to form hard nickel beryllides which function similar to the carbide mechanism in Cr-Mo-V and Cr-W-V aBoy steels...
Journal Articles
Alloy Digest (1964) 13 (3): Ni-89.
Published: 01 March 1964
... and resistance. For metal-arc welding use Nickel Welding Electrode 141 with &he work made the negative electrode. Nickel Filler Metal 61 is used for TIG and MIG welding; the shielding or purge gas should be argon. helium or a mixture of tbe two. For oxyacetylene welding, Nickel Filler Metal 41 is used...
Journal Articles
Alloy Digest (1968) 17 (10): Ni-139.
Published: 01 October 1968
... electrode. Nickel Filler Metal 61 wire is used for inert-gas metal-arc welding. The oxyacetylene process is not applicable to Nickel-201. Typical creep strength of annealed Nickel 201. Corrosion Resistwce: In general, it is much more susceptible to corrosion in a oxidizing atmosphere ot by an oxidizing...
Journal Articles
Alloy Digest (1967) 16 (8): Ni-126.
Published: 01 August 1967
... and Nickel Filler Metal 61 for inert-gas metallic-arc welding. Corrosion Resistance: Very high resistance to all kinds of corrosive media, except a sulphurous condition. Will resist alkalis, mineral acids and organic acids, but not oxidizing acids ot oxidizing salts. Nitric acid readily attacks Permanickel...
Journal Articles
Alloy Digest (1984) 33 (9): Ni-302.
Published: 01 September 1984
... INCONEL Filler Metal 617 is a nickel-base alloy suitable for welding a number of alloys. It is used for the gas tungsten-arc (TIG) and gas metal-arc (MIG) welding of INCONEL alloy 617. For extended service at temperatures above 1700 F (925 C), it is recommended for welding INCOLOY alloy 800H...
Journal Articles
Alloy Digest (1992) 41 (7): Ni-407.
Published: 01 July 1992
... Filing Code: Nickel Alloy NM07 - DIGEST- JULY 1992 DATA ON WORLD WIDE METALS AND ALLOYS ec@Jy@f 1992, Amy QJaBl, k. Aur.ghts r(LBBNed. PlMishdby: Aloy Digsa. IK I2ola7-9161 apbs~~wmbe~fw 27Cadi~kISoeqOr~NJ.07050lU.S.A INCONEL WELDING ELECTRODE 122 (Pittlng and Crevice Corrosion Resistant Nickel-Base...
Journal Articles
Alloy Digest (2002) 51 (9): Ni-590.
Published: 01 September 2002
..., and stress-corrosion cracking. In addition to welding the parent alloy 617, some authorities spec- ify Rima 617 in preference to other nickel-base filler metals for welding alloys 800H and 800HT for service above 760 °C (1400 °F). It is also suitable for the heat-resistant alloy 601 (usually above 900 °C...
Journal Articles
Alloy Digest (1988) 37 (11): Ni-364.
Published: 01 November 1988
... of the mol- ten weld metal necessitates joint design sufficiently open toallow full filler wire access to fill the joint. High thermal conductivity results in lower weld penetration than with austenitic stainless steels. Stabilized nickel-base fillers such as Nickel Electrode 14 1, Nickel 61 or Into-Weld...
Journal Articles
Alloy Digest (1993) 42 (5): Ni-432.
Published: 01 May 1993
... International Inc. Copyright © ASM International® 1996 1996 ASM International cast nickel alloys chemical composition corrosion-resistant alloys elasticity fracture toughness G-30 FILLER METAL joinability physical properties tensile properties wrought nickel alloys thermal properties UNS...
Journal Articles
Alloy Digest (2021) 70 (5): SS-1335.
Published: 01 May 2021
... metals are suggested for welding ATI 2003. 149 300 32 Such filler metals (AWS E2209) contain more nickel than the 204 400 662 96 889 129 27 base metal in order to produce a phase balance within the 260 500 26 weld that is approximately the same as the base metal. When 614 89 820 119 22 ATI 2003 LDSS...
Journal Articles
Alloy Digest (2005) 54 (3): Ni-624.
Published: 01 March 2005
... be by gas tungsten arc, gas metal arc, and shielded metal arc processes. Matched composition welding products, such as Inconel Welding Electrode 122 and Filler Metal 622, are available. Overmatching composition welds may be deposited with Inco-Weld Filler Metal 686CPT or Inco-Weld Welding Electrode 686CPT...
Journal Articles
Alloy Digest (1972) 21 (6): SA-276.
Published: 01 June 1972
... 5 steel can be welded with austenitic nickel-chromium alloy fffler metals, such as INCO-WELD* A or INCONEL* Filler Metal 92. Reheating ordinarily is unnecessary except for welding joints in heavy or highly restrained members; a temperature of 200 to 4000F usually is applied to joints of this type...
Journal Articles
Alloy Digest (2009) 58 (1): SS-1028.
Published: 01 January 2009
... and properties, overalloyed filler materials are recommended (nickel and/or nitrogen additions). Excessive dilutions must be avoided. Filler materials and shielding gases guaranteeing PREN > 40 have been developed (wire, metallic cored wire, electrodes). A list of tested filler materials is available on request...