Alloy Digest (1975) 24 (1): Ni-214.
Published: 01 January 1975
... Nickel-Copper Alloys 410 and 411 are strong and ductile casting alloys; they are generally used in conjunction with wrought counterparts. They can be cast readily into fittings such as elbows, tees, return bends, flanges and similar components. This datasheet provides information on composition...
Journal Articles
Alloy Digest (2009) 58 (11): Fe-149.
Published: 01 November 2009
... Bimetal) KANTHAL® 180 R05 Chemical Composition, wt (Nominal) High-expansive component 411 Low-expansive component 450 Manganese 74 0.12 Nickel 12 36.8 Copper 14 Iron bal bal Physical Properties: Density, kg/m3 (lb/in.3) 8200 (0.295) Electrical resistivity, bimetal, Designation 180 R05, · m ( circular...
Journal Articles
Alloy Digest (2008) 57 (5): Mn-4.
Published: 01 May 2008
...- expansive component Intermediate component Designation 411 450 470 Manganese 74 0.12 Nickel 12 36.8 Copper 14 100 Iron bal Portion of 43.5 38.7 17.8 thickness, % Marking on the high expansion side: 200R10TB2010 Physical Properties: Density, kg/m3 (lb/in.3) 7900 (0.285) Coefficient of linear thermal...
Journal Articles
Alloy Digest (2008) 57 (2): Mn-3.
Published: 01 February 2008
... Designation 411 430 Manganese 74.0 0.30 Nickel 11.5 36.5 Copper 14.0 Iron bal Physical Properties: (Marking on the high expansion side 210TB20220) Density, kg/m3 (lb/in.3) 7800 (0.282) Coefficient of linear thermal expansion, 35 120 °C (95 248 °F), 10 6/K (10 6/°F) High-expansive component 411 27.3 (15.2) Low...
Journal Articles
Alloy Digest (1966) 15 (6): Cu-164.
Published: 01 June 1966
... CUNISIL-647 is a copper-nickel-silicon precipitation-hardening alloy having high strength, hardness, wear and corrosion resistance. Typical applications include electrical hardware and fasteners. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (1982) 31 (7): SS-411.
Published: 01 July 1982
... CRONIFER 2328 is a titanium-stabilized, high-chromium and high-nickel austenitic stainless steel with additions of molybdenum and copper. It exhibits good corrosion resistance against sulfuric and phosphoric acids. Also, it has good resistance against pitting and stress-corrosion cracking...
Journal Articles
Alloy Digest (2002) 51 (7): Cu-685.
Published: 01 July 2002
... Swissmetal alloy SM468C is a heat treatable copper alloy with high strength and hardness. It has good corrosion resistance and relatively good conductivity. It is used in electrical generators. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (1985) 34 (9): Ni-321.
Published: 01 September 1985
... is a registered trademark of the Into family of companies. Composition: Limiting for Deposited Filler Metal Nickel (+ Cobalt) Carbon Manganese Iron Sulfur Silicon Copper Aluminum Titanium Phosphorus Others 62.0-69.0 0.15 max. 4.0 max. 2.5 max. 0.015 max. I .O max. Remainder 0.75 max. 1.0 max. 0.02 max. 0.50 max...
Journal Articles
Alloy Digest (1967) 16 (9): Ni-127.
Published: 01 September 1967
... CM-R41 is a vacuum-melted, precipitation hardening nickel-base alloy possessing outstanding properties in the temperature range of 1200 F to 1800 F. It is recommended for jet engine and gas turbine components operating at high temperatures. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1998) 47 (9): Ni-545.
Published: 01 September 1998
... No. $183,636. Chemical Composition, wL%: (Nominal) Chromium Boron Silicon Copper Molybdenum Columbium Carbon Nickel 7.9 2 ::2 2.5 2.0 2.0 co.06 Balance bonded overlay becomes a dense, fused, metahurgically bonded overlay. Inspection by heat checking the overlay may be done to test bond integrity. Safety...
Journal Articles
Alloy Digest (2000) 49 (11): Cb-25.
Published: 01 November 2000
... Inc. Chemical Composition, wt%: Element Composition, wt.% Hafnium 10.0 Titanium 0.7 1.3 Zirconium 0.7 Tantalum 0.5 Tungsten 0.5 Element Guaranteed impurity, ppm Carbon <150 Hydrogen <10 Iron <50 Copper <40 Chromium <20 Manganese <20 Nickel <20 Vanadium <20 Tin <10 Oxygen <225 Nitrogen <150 Silicon <50...
Journal Articles
Alloy Digest (1987) 36 (1): SS-481.
Published: 01 January 1987
.... .. Composition: Carbon 0.04 max. Manganese 1.5 max. Phosphorus 0.04 max. Sulfur 0.03 max. Silicon I .O max. Chromium 24.0-27.0 Nickel 4.5-6.5 Molybdenum* 2.9-3.9 Copper I S-2.5 Nitrogen 0. I O-O.25 Iron Remainder *Even lmum thmooulyg.aha.en.AuSmT,M st.pn.eecifiemsanu2t.a0cr%turemr in- uses 2.9k minimum...